1. Starting with a sketch and a clay model of the handle.
-
2. The clay model has been dipped in molten Dip Seal, then the Dip Seal rubbery coating cut with a sharp knife and removed.
-
3. The rubbery pattern has been spread flat and traced onto paper, the resulting paper pattern then traced onto 81 gauge brass sheet.
-
4. Starting the forming process.
-
5. The seam is silver-soldered a little bit at a time.
-
6. After first silver-soldering, I continue spiraling it around. Here is a special stake that I made, shown at the top, for forming this part of it.
-
7. Forming the little pointed end.
-
8. Using another special stake to form the roundness of the bottom end.
-
9. It needed to be annealed again in order to get final closure of the form.
-
10. Final closure.
-
11. The last part of the seam has been silver-soldered.
-
12. Bending and forming the curly-Q at the end.